Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 24.46 J/cm @Temperature -40.0 °C |
45.82 ft-lb/in @Temperature -40.0 °F |
ASTM D4812 |
Eastman Eastar MN058 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN058 Copolyester is a medical gra.. |
|||
Izod Impact, Unnotched | 24.46 J/cm @Temperature -40.0 °C |
45.82 ft-lb/in @Temperature -40.0 °F |
ASTM D4812 |
Eastman Eastar MN059 Copolyester Eastar copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN059 Copolyester is a medical gra.. |