Izod Impact, Unnotched 24.0 J/cm

@Temperature -40.0 °C
45.0 ft-lb/in

@Temperature -40.0 °F
ASTM D4812
Eastman Eastar EN010 Copolyester
Eastar copolyester EN010 is used primarily in molded thick wall European applications.Applications/UsesPackagingInjection moldingContainers