Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 43.7 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 23.3 J/cm
43.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DX98477 PC
LNP* STAT-KON* DX98477 is a compound based on Polycarbonate containing Proprietary Filler(s). Added feature of this grade is: Electrically Conductive.
Copyright © lookpolymers.com All Rights Reserved