Mechanical Properties Metric English Comments
Izod Impact, Unnotched 22.26 J/cm
41.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD000P PC
LNP* STAT-KON* DD000P is a compound based on Polycarbonate resin containing Carbon. Added features of this material include: Electrically Conductive, Exceptional Processing.
Izod Impact, Unnotched 22.26 J/cm
41.70 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON DD000P PC (Asia Pacific)
LNP* Stat-kon* DD000P is a compound based on Polycarbonate resin containing Carbon Powder. Added features of this material include: Electrically Conductive, Exceptional Processing.