Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.98 J/cm | 9.33 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF004P PES (Asia Pacific) LNP* Thermocomp* JF004P is a compound based on Polyethersulfone resin containing Glass Fiber. Added features of this material include: Exceptional Processing. |
|||
Izod Impact, Unnotched | 4.98 J/cm | 9.33 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP JF004P PES LNP* THERMOCOMP* JF004P is a compound based on Polyethersulfone resin containing 20% Glass Fiber. Added features of this material include: Exceptional Processing. |