Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.46 J/cm
4.61 ft-lb/in
ASTM D256
A. Schulman ComAlloy Voloy® 612 Nylon 6, Glass Fiber/Bead Reinforced, Flame Retardant, UL
Data provided by the manufacturer, ComAlloy International Company.30% Glass Fiber/Bead Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.
Izod Impact, Unnotched 2.46 J/cm
4.61 ft-lb/in
ASTM D256
A. Schulman ComAlloy Hiloy® 221 ABS, Glass Reinforced, UL
Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line.