Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 4.61 J/cm | 8.64 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,.. |
|||
Izod Impact, Unnotched | 4.61 J/cm | 8.64 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP UFL269SA PPA (Asia Pacific) LNP* Lubricomp* UFL269SA is a compound based on Polyphthalamide resin containing Glass Fiber, PTFE, Flame Retardant. Added features of this material include: Internally Lubricated, Heat Stabilized,.. |