Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 20.29 J/cm @Temperature 23.0 °C |
38.01 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics Valox® 308 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Unnotched | 20.29 J/cm | 38.01 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 309 PBT PBT, For compounding only. Not intended for Injection Molding. Melt viscosity: 250C at 21.6 kgf is 3500-4500. Available in Natural (1001) only. |