Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 20.2 J/cm | 37.8 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP DL0029E PC LNP LUBRICOMP* DL0029E is a compound based on Polycarbonate resin containing 10% PTFE. Added features of this material include: Internally Lubricated, Flame Retardant. |