Mechanical Properties Metric English Comments
Izod Impact, Unnotched 8.00 - 20.0 J/cm
15.0 - 37.5 ft-lb/in
Low Temp; ASTM D256
Solvay Specialty Polymers Hylar® 460 PVDF Polyvinylidene Fluoride  (discontinued **)
Data provided by the manufacturer.Hylar® polymers have the characteristic stability of fluoropolymers combined with a unique polarity that influences its solubility and electrical properties. In a..