Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 19.75 J/cm | 37.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC LNP* LUBRILOY* D20009P is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added features of this material include: Wear Resistant, Flame Retardant, Exceptional Processing... |
|||
Izod Impact, Unnotched | 19.75 J/cm | 37.00 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRILOY D20009P PC (Asia Pacific) LNP* Lubriloy* D20009P is a compound based on Polycarbonate resin containing Flame Retardant, Proprietary Lubricant. Added features of this material include: Internally Lubricated, Flame Retardant,.. |