Mechanical Properties Metric English Comments
Izod Impact, Unnotched 18.16 J/cm
34.02 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF50 - PA66 MT Nylon 66, 50% Long Glass Fiber Reinforced, Impact Modified
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Nylon 6 with 50% long glass fiber reinforcementImpact modifiedInformation provided by ..