Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 3.91 J/cm | 7.33 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP OF006 PPS - Linear LNP* THERMOCOMP* OF006 is a compound based on Linear PPS containing 30% Glass Fiber. |