Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON MD000IS PP LNP STAT-KON* MD000IS is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP (Asia Pacific) LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing 20% PTFE. Added feature of this material is: Wear Resistant. |
|||
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Asia Pacific) LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP LL004 PEEK (Europe-Africa-Middle East) LNP LUBRICOMP* LL004 is a compound based on Polyetheretherketone resin containing PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 15.53 J/cm | 29.09 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON MD000ISC PP LNP STAT-KON* MD000ISC is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |