Polymer Property : Izod Impact, Unnotched = 27.2 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 14.5 J/cm

@Temperature -30.0 °C
27.2 ft-lb/in

@Temperature -22.0 °F
ASTM D4812
SABIC Innovative Plastics Cycoloy® CM8622 PC+ABS (Europe-Africa-Middle East)
CYCOLOY* CM8622 is a high heat PC/ABS blend offering high modulus, low CTE and good