Mechanical Properties Metric English Comments
Izod Impact, Unnotched 14.3 J/cm

@Thickness 3.18 mm
26.8 ft-lb/in

@Thickness 0.125 in
ASTM D256
LNP Thermocomp® HF-1006 Polyamide 11, Glass Fiber Reinforcement  (discontinued **)
Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names..