Polymer Property : Izod Impact, Unnotched = 23.0 ft-lb/in Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
ASTM D-4812
PlastiComp Velocity® LGF50-PA66 High Flow Nylon 66, 50% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
ASTM D-4812
PlastiComp Velocity® LGF60-PA66 High Flow Nylon 66, 60% Long Glass Fiber
This compound complies with European Union Directive 2002/95/EC Restriction of Hazardous Substances (RoHS).Information provided by PlastiComp, Inc.
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
Reliance Industries Polypropylene - Calcium carbonate filled
Information provided by Reliance Industries
Izod Impact, Unnotched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF60 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightProcessing Method: Injection MoldingInformation provided by TP Composites, Inc.
Izod Impact, Unnotched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF60 HS L 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Heat Stabilized and LubricatedInformati..
Izod Impact, Unnotched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF60 HS L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: Heat StabilizerFeatures: Heat StabilizedAppearance: BlackProcessing Method: In..
Izod Impact, Unnotched 12.3 J/cm

@Thickness 3.17 mm
23.0 ft-lb/in

@Thickness 0.125 in
ASTM D256
Techmer ES HiFill® PA6 GF60 L BK 60% Glass Filled
Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 60% Filler by WeightAdditive: LubricantFeatures: LubricatedAppearance: BlackInformation provided by TP Compo..
Izod Impact, Unnotched 12.3 J/cm
23.0 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP TF002 PU
LNP* THERMOCOMP* TF002 is a compound based on Polyurethane resin containing 10% Glass Fiber.