Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.4 J/cm | 21.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX98372H PA 66 LNP* Thermocomp* RX98372H is a compound based on Nylon 66 resin containing Proprietary Fillers. Characteristics of this grade are: Healthcare. |
|||
Izod Impact, Unnotched | 11.4 J/cm @Temperature 23.0 °C |
21.4 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton RV008ESV PA 66 40% long glass fiber filled PA66 Verton Xtreme XCThis data was supplied by SABIC-IP for the Americas region. |