Mechanical Properties Metric English Comments
Izod Impact, Unnotched 20.34 J/cm

@Temperature 23.0 °C
38.11 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Lubriloy Z2000 PPE+PS
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC-IP fo..
Izod Impact, Unnotched 20.34 J/cm
38.11 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPE+PS (Asia Pacific)
LNP* Lubriloy* Z2000 is a compound based on PPE+PS Blend resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 20.34 J/cm
38.11 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRILOY Z2000 PPO
LNP* LUBRILOY* Z2000 is a compound based on PPO resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Copyright © lookpolymers.com All Rights Reserved