Polymer Property : Izod Impact, Unnotched = 2.93 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 2.93 J/cm
5.49 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP KFL25 Acetal Copolymer
LNP LUBRICOMP* KFL25 is a compound based on Acetal Copolymer resin containing 25% Glass Fiber, 10% PTFE. Added feature of this material is: Wear Resistant.
Izod Impact, Unnotched 2.93 J/cm
5.49 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP WL0049 PBT
LNP* LUBRICOMP* WL0049 is a compound based on PBT containing 20% PTFE. Added features include: Wear Resistant, Flame Retardant.
Izod Impact, Unnotched 2.93 J/cm

@Temperature 23.0 °C
5.49 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812
SABIC Innovative Plastics LNP Thermocomp KB005 Acetal Copolymer
LNP THERMOCOMP* KB005 is a compound based on Acetal Copolymer resin containing Glass Bead.This data was supplied by SABIC-IP for the Americas region.
Izod Impact, Unnotched 2.93 J/cm
5.49 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP MX06403 PP
LNP* THERMOCOMP* MX06403 is a compound based on Polypropylene resin containing 20% Glass Fiber. Added features of this material include: Heat Stabilized, UV Stabilized.