Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
Hyosung Topilene B201Y PP B201Y Extrusion Special Purpose GradeApplications:Thermoforming sheetExtrusion blow moldingCharacteristics:Low smellFormabilityInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |
Hyosung Topilene J340 PP J340 Injection Impact CopolymerApplications:CrateContainerBatter caseCharacteristics:High ImpactInformation provided by Hyosung Corporation |
|||
Izod Impact, Unnotched | 1.47 J/cm | 2.76 ft-lb/in | ASTM D256 |