Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.801 - 1.33 J/cm
1.50 - 2.50 ft-lb/in
ASTM D256
CPC - Vycom FLAMETEC™ KYTEC® PVDF
Kytec® PVDF, the homopolymer of 1, 1-difluoroethene, is a tough engineering thermoplastic that offers a unique balance of properties. Kytec has the characteristic stability of fluoropolymers when e..