Polymer Property : Izod Impact, Unnotched = 2.27 J/cm
Polymer Property :
Izod Impact, Unnotched =
2.27 J/cm
Product List
Mechanical Properties
Tips:
30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties
Metric
English
Comments
Izod Impact, Unnotched
2.27
J/cm
4.25
ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP RB004 PA 66
LNP* THERMOCOMP* RB004 is a compound based on Nylon 66 containing Glass Beads.