Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.13 J/cm @Temperature 23.0 °C |
3.99 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Lubricomp RP0049 PA 66 LNP LUBRICOMP* RP0049 is a compound based on Nylon 66 resin containing Flame Retardant, PTFE, Silicone. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP f.. |
|||
Izod Impact, Unnotched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 LNP* STAT-KON* RFD02 is a compound based on Nylon 66 resin containing 10% Glass Fiber. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RFD02 PA 66 (Asia Pacific) LNP* Stat-kon* RFD02 is a compound based on Nylon 66 resin containing Glass Fiber, Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Izod Impact, Unnotched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D256 |
ALM PA 614-GS Filled Nylon 12 Prototyping Polymer 40% glass sphere filled material for improved dimensional stability, increased stiffness, and higher temperature applications when compared to unfilled PA.Drop-in replacement for other commercially .. |
|||
Izod Impact, Unnotched | 2.13 J/cm | 3.99 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON ME006 PP (Asia Pacific) LNP STAT-KON* ME006 is a compound based on Polypropylene resin containing Carbon Fiber. Added features of this material include: Electrically Conductive. |