Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 2.02882 - 2.1356 J/cm @Temperature -18.0 - -18.0 °C |
3.80081 - 4.0009 ft-lb/in @Temperature -0.400 - -0.400 °F |
Average value: 2.06 J/cm Grade Count:3 |
Overview of materials for Polypropylene, Extrusion Grade This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Extrusion Grade". Each property range of values reported is minimum and maximum values of.. |