Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 10.65 J/cm

@Temperature 23.0 °C
19.95 ft-lb/in

@Temperature 73.4 °F
DAM; ASTM D4812
DuPont Performance Polymers Zytel® 77G33L BK031 Nylon 612  (Unverified Data**)
Zytel® 77G33L BK031 is a 33% glass fiber reinforced, black polyamide 612 resin for injection molding.Information provided by DuPont Performance Polymers
Izod Impact, Unnotched 10.65 J/cm
19.95 ft-lb/in
ASTM D256A
Total PPH 3720WZ Polypropylene, Injection Molding Grade
High flow reactor injection molding homopolymerHigh Flow - FINA 3720WZ has high flow characteristics that result in ease of filling thin wall parts.Nucleation - FINA 3720WZ is nucleated to provide f..
Izod Impact, Unnotched 10.65 J/cm
19.95 ft-lb/in
ASTM D256A
Total PPH 3721WZ Polypropylene, Injection Molding Grade
High flow reactor homopolymer with a high level of antistatHigh Flow - FINA 3721WZ is designed with high flow characteristics for ease of filling thin wall parts.High Antistat - FINA 3721WZ is engin..