Mechanical Properties Metric English Comments
Izod Impact, Unnotched 10.2 J/cm
19.1 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP PX01658 PA 6
LNP* Thermocomp* PX01658 is a compound based on Nylon 6 containing Proprietary Fillers.