Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 18.1 J/cm | 33.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |