Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 9.13 J/cm @Thickness 3.18 mm |
17.1 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® LF-1006 EM Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |
|||
Izod Impact, Unnotched | 9.11 J/cm | 17.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFP38 PA6.6 LNP* LUBRICOMP* RFP38 is a compound based on Nylon 66 containing 40% Glass Fiber, 15% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Izod Impact, Unnotched | 9.14 J/cm | 17.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF006LXN PC LNP* THERMOCOMP* DF006LXN is a compound based on Polycarbonate resin containing 30% Glass Fiber. Added features of this material are: Low Extractable, NSF Listed. |
|||
Izod Impact, Unnotched | 9.13 J/cm | 17.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF006E PEEK LNP* THERMOCOMP* LF006E is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. Added features of this material include: Easy Molding. |
|||
Izod Impact, Unnotched | 9.14 J/cm | 17.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP DF006 PC LNP* Thermocomp* DF006 is a compound based on Polycarbonate resin containing 30% Glass Fiber. |