Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.98 J/cm
31.81 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS
LNP* STAT-LOY* A30009 is a compound based on ABS. Added features of this material include: Antistatic, Flame Retardant.
Izod Impact, Unnotched 16.98 J/cm
31.81 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY A30009 ABS (Asia Pacific)
LNP* Stat-loy* A30009 is a compound based on Acrylonitrile Butadiene Styrene resin containing Flame Retardant. Added features of this material include: Antistat, Flame Retardant.