Polymer Property : Izod Impact, Unnotched = 16.9 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.9 J/cm
31.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-LOY 9X07438 ASA+PC
LNP* STAT-LOY* 9X07438 is a compound based on Polycarbonate/ASA containing Proprietary Filler(s). Added features of this grade include: Antistatic, Colorable, Weatherable.