Polymer Property : Izod Impact, Unnotched = 16.55 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.55 J/cm
31.00 ft-lb/in
ASTM D-4812
PlastiComp Complet® LGF60 - TPU Rigid Thermoplastic Polyurethane, 60% Long Glass Fiber Reinforced
Complēt® long-fiber reinforced pellets are manufactured to exceed expectation for quality and performance.Rigid polyurethane with 60% long glass fiber reinforcementInformation provided by Plas..