Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.75 J/cm @Thickness 3.18 mm |
16.4 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
LNP Thermocomp® LF-1006 Polyetheretherketone, Glass Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
Izod Impact, Unnotched | 8.75 J/cm | 16.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF006 PEEK LNP THERMOCOMP* LF006 is a compound based on Polyetheretherketone resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched | 8.76 J/cm | 16.4 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOTUF PX95726 PA 6 LNP THERMOTUF* PX95726 is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: Heat Stabilized. |