Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Unnotched = 16.4 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 16.4 J/cm
30.7 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 9X10401H ABS
LNP* THERMOCOMP* 9X10401H is a compound based on Polyphenylsulfone containing proprietary filler(s). Added feature of this grade is: X-Ray Opaque.
Izod Impact, Unnotched 16.4 J/cm
30.7 ft-lb/in
ASTM Test
BASF Ultramid® 8260 40% Mineral Filled PA6 (Dry)
Ultramid 8260 is a 40% mineral reinforced PA6 injection molding compound. It possesses high stiffness, dimensional stability and heat resistance combined with excellent processability including low..