Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 16.23 J/cm | 30.41 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP STAT-KON DX00887C PC LNP STAT-KON* DX00887C is a compound based on Polycarbonate resin containing Proprietary Filler(s). Added features of this material include: Clean Compounding System, Electrically Conductive. |