Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 8.61 J/cm | 16.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP LFL36E PEEK LNP* LUBRICOMP* LFL36E is a compound based on Polyetheretherketone containing 30% Glass Fiber, 15% PTFE. Added features of this material are: Wear Resistant, Easy Molding. |
|||
Izod Impact, Unnotched | 8.60 J/cm | 16.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP LF002 PEEK LNP* THERMOCOMP* LF002 is a compound based on Polyetheretherketone resin containing 10% Glass Fiber. |
|||
Izod Impact, Unnotched | 8.57 J/cm | 16.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 430 PBT 33 % glass reinforced, impact modified. Connectors, etc. |
|||
Izod Impact, Unnotched | 8.57 J/cm | 16.1 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics Valox® 430 PBT (Asia Pacific) 33 % glass reinforced, impact modified. Connectors, etc. |