Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 14.75 J/cm @Temperature 23.0 °C |
27.63 ft-lb/in @Temperature 73.4 °F |
ASTM D 4812 |
SABIC Innovative Plastics LNP Verton RX93407D PA 66 (Asia Pacific) LNP* Verton* RX93407D is a compound based on Nylon 66 resin.This data was supplied by SABIC-IP for the Asia Pacific region. |