Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 12.2 J/cm | 22.9 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP RX00713H PA 66 LNP* Thermocomp* RX00713H is a compound based on Nylon 6/6 containing proprietary fillers. Characteristics of this grade are: Healthcare. |