Mechanical Properties Metric English Comments
Izod Impact, Unnotched 6.138 J/cm
11.50 ft-lb/in
Method A; ASTM D256
Proto3000 ULTEM* 9085 Fused Deposition Modeling Polymer
Description: ULTEM* 9085 is a flame retardant high performance thermoplastic for direct digital manufacturing and rapid prototyping. It is ideal for the transportation industry due to its high stren..