Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 11.05 J/cm | 20.70 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP THERMOCOMP PF008QS PA 6 LNP THERMOCOMP* PF008QS is a compound based on Nylon 6 resin containing 40% Glass Fiber. Added features of this material include: Heat Stabilized, Reduced Moisture. |