Mechanical Properties Metric English Comments
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP LUBRICOMP FL004 PE
LNP* Lubricomp* FL004 is a compound based on Polyethylene resin containing 20% PTFE. Added features of this material include: Internally Lubricated.
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE006 PA 66
LNP STAT-KON* RE006 is a compound based on Nylon 66 resin containing 30% Carbon Fiber. Added features of this material include: Electrically Conductive.
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE007 PA 66
LNP* STAT-KON* RE007 is a compound based on PA66 resin containing 35% Carbon Fiber. Added features include: Electrically Conductive.
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D256
A. Schulman ComAlloy Comtuf® 102 Polypropylene, Mineral Reinforced, Impact Modified
Data provided by the manufacturer, ComAlloy International Company.20% Mineral Reinforced. Superior toughness and impact resistance characterize Comtuf® materialsThe ComAlloy product line has been i..
Izod Impact, Unnotched 10.3 J/cm
19.3 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP 2X04505 ETFE
LNP* THERMOCOMP* 2X04505 is a compound based on ETFE resin containing Proprietary Filler(s).