Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 10.04 J/cm | 18.81 ft-lb/in | ASTM D-4812 |
PlastiComp Complet® LCF20/LGF20 – PA66 BLK Polyamide 66, 40% Long Carbon/Glass Fiber Composite PelletsInformation provided by PlastiComp, Inc. |
|||
Izod Impact, Unnotched | 10.04 J/cm | 18.81 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16 PA 6 LNP* LUBRICOMP* RFN16 is a compound based on Nylon 66 resin containing 30% Glass Fiber, 5% MOS2. Added features of this material include: Wear Resistant. |
|||
Izod Impact, Unnotched | 10.04 J/cm | 18.81 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP RFN16 PA 6 (Asia Pacific) LNP* Lubricomp* RFN16 is a compound based on Nylon 6 resin containing Glass Fiber, MOS2. Added features of this material include: Internally Lubricated. |