Polymer Property : Izod Impact, Unnotched = 10.0 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 4.30 - 10.0 J/cm
8.06 - 18.7 ft-lb/in
Average value: 7.86 J/cm Grade Count:10
Overview of materials for Polyaryletherketone (PAEK), Glass Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polyaryletherketone (PAEK), Glass Fiber Filled". Each property range of values reported is minimum and m..
Izod Impact, Unnotched 4.59 - 10.0 J/cm
8.60 - 18.8 ft-lb/in
Average value: 7.76 J/cm Grade Count:5
Overview of materials for Nylon 66, Glass/Carbon Fiber Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Glass/Carbon Fiber Filled". Each property range of values reported is minimum and maximum valu..