Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.550 - 0.950 J/cm @Temperature 23.0 °C |
1.03 - 1.78 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 912 Rigid PVC, Extrusion Lead Free Spiral pipes |