Polymer Property : Izod Impact, Unnotched = 1.55 J/cm Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.55 J/cm
2.90 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP THERMOCOMP CX05470 PS (Asia Pacific)
LNP* Thermocomp* CX05470 is a compound based on Polystyrene resin containing Glass Fiber.
Izod Impact, Unnotched 1.55 J/cm
2.90 ft-lb/in
ASTM D256
Wico Plast Wicoran 57 ABS, High Gloss
ApplicationsInjection moldingCharacteristics:High glossAll information provided by Wico Plast, Warenhandelsges. mbH