Mechanical Properties Metric English Comments
Izod Impact, Unnotched 1.06 J/cm
1.99 ft-lb/in
ASTM D4812
SABIC Innovative Plastics LNP STAT-KON RE006 PA6.6 (Asia Pacific)
LNP STAT-KON RE006 is a compound based on Nylon 66 containing carbon fiber. Added features of this material include: Electrically Conductive. Also known as STAT-KON RC-1006