Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 410 Rigid PVC, Extrusion Clic channels |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 412/L Rigid PVC, Extrusion Corrugated plastics |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 520/1 Rigid PVC, Extrusion Electric pipes |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 218 Rigid PVC, Extrusion Lead Free Rolling shutters |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RK 321 Rigid PVC, Extrusion Lead Free Profiles |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 130 Rigid PVC, Extrusion Pipes and profiles |
|||
Izod Impact, Unnotched | 0.500 - 0.900 J/cm @Temperature 23.0 °C |
0.937 - 1.69 ft-lb/in @Temperature 73.4 °F |
ISO R180 |
Fainplast Compounds RE 140/1 Rigid PVC, Extrusion Drain-pipes |