Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.760 J/cm | 1.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS (Asia Pacific) LNP* Lubricomp* CBL36XXC is a compound based on Polystyrene resin containing Glass Bead, PTFE. Added features of this material include: Internally Lubricated. |
|||
Izod Impact, Unnotched | 0.760 J/cm | 1.42 ft-lb/in | ASTM D4812 |
SABIC Innovative Plastics LNP LUBRICOMP CBL36XXC PS LNP* LUBRICOMP* CBL36XXC is a compound based on Polystyrene resin containing 30% Glass Bead and 15% PTFE. Added features of this material include: Wear Resistant. |