Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched | 0.294 J/cm @Temperature -40.0 °C |
0.550 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Spartech Solarex® SV Copolyester Sheet Description: Copolyester SheetInformation provided by Spartech. |