Mechanical Properties Metric English Comments
Izod Impact, Unnotched 0.290 J/cm - NB
0.543 ft-lb/in - NB
Average value: 11.4 J/cm Grade Count:26
Overview of materials for Polycarbonate, 10% Glass Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea..
Izod Impact, Unnotched 0.290 J/cm
0.543 ft-lb/in
ASTM Data
Styron CALIBREâ„¢ 5101 15 Polycarbonate, 10% Glass Reinforced
CALIBRE 5101 is a 10% glass reinforced polycarbonate resin containing mold release for optimal processing. CALIBRE 5101 resin exhibits high modulus and excellent dimensional stability. CALIBRE 5101 ..